| Property | Test Method | Test Value |
|---|---|---|
| Tensile Strength | ASTM D2671 | ≥12MPa |
| Elongation at Break | ASTM D2671 | ≥350% |
| Elongation at Break After Aging | ASTM D2671 (150°C/168 hours) |
≥12MPa |
| Dielectric Strength | ASTM D2671 (150°C/168 hours) |
≥300% |
| Volume Resistivity | ASTM D2671 | ≥10kV/mm |
| Copper Stability | ASTM D2671 | ≥10^12 Ω·cm |
| Flammability | UL224 | Pass (outer layer VW-1) |
| Hot-Melt Adhesive | ||
| จุดอ่อนตัว | ASTM E28 | 85±5°C |
| Water Absorption | ISO 62 | ≤0.2% |
| ความต้านทานการลอกออกของกาว (PE) | DIN 30672 | ≥4N/cm |
| Product Code | Before Shrinking(mm) | After Shrinking (mm) | Standard Length (m) | |
|---|---|---|---|---|
| I.D. (min) | I.D. (max) | W.T. (min) | ||
| ATMFR022 | 8 | 2 | 1.7 | 1.22 |
| ATMFR033 | 12 | 4 | 2.0 | 1.22 |
| ATMFR040 | 16 | 5 | 2.2 | 1.22 |
| ATMFR055 | 19 | 5 | 2.2 | 1.22 |
| ATMFR065 | 22 | 6 | 2.5 | 1.22 |
| ATMFR075 | 28 | 6 | 2.5 | 1.22 |
| ATMFR095 | 33 | 8 | 2.5 | 1.22 |
| ATMFR115 | 40 | 12 | 2.5 | 1.22 |
| ATMFR140 | 44 | 14 | 2.5 | 1.22 |
| ATMFR160 | 55 | 16 | 2.7 | 1.22 |